Thermoelectric and mechanical performances of ionic liquid-modulated PEDOT:PSS/SWCNT composites at high temperatures

Figure 5. Typical scanning electronic microscopy images of PEDOT:PSS/SWCNT-IL composites with a SWCNT content of 30 (Row I) or 60 wt.% (Row II) after TE test at (A, C) room temperature and (B, D) after TE test at 470 K. PEDOT:PSS/SWCNT: Poly(3,4-ethylenedioxythiophene):poly(styrene sulfonate)/single-walled carbon nanotube; IL: ionic liquid.