Improved thermoelectric performance in n-type flexible Bi<sub>2</sub>Se<sub>3+x</sub>/PVDF composite films

Figure 2. (A, B) XRD patterns of the Bi2Se3+x/PVDF composite films; (C) XPS spectra fitting curve for Bi2Se3.2 powder; and (D) Se/Bi molar ratio of ICP-MS measurement for Bi2Se3+x (x = 0, 0.2, 0.3, 0.4) powder.